Fabrication and Electrothermal Anti-Icing/De-Icing Performance of Composite Leading Edges With CNTs
RESEARCH | 更新时间:2026-09-23
    • Fabrication and Electrothermal Anti-Icing/De-Icing Performance of Composite Leading Edges With CNTs

    • Aeronautical Manufacturing Techinology   Vol. 69, Issue 17, (2026)
    • DOI:10.16080/j.issn1671-833x.26010013    

      CLC: V244.1+5;V25;TB33
    • Received:12 January 2026,

      Revised:2026-02-04,

      Accepted:27 February 2026,

      Published:01 September 2026

    移动端阅览

  • WANG Haolin, YING Yuxuan, WANG Li, et al. Fabrication and electrothermal anti-icing/de-icing performance of composite leading edges with CNTs[J]. Aeronautical Manufacturing Technology, 2026, 69(17): 26010013. DOI: 10.16080/j.issn1671-833x.26010013.

  •  
  •  

0

Views

0

下载量

0

CSCD

Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Research on Influence of Assembly Gap on Secondary Bending Effect of CFRP–Al Bolted Joint Structures
Study on Influencing Factors and Mechanisms of Curing Deformation in U-Shaped Composite Long Beam Components
Design and Verification of the Hot-Press Scheme for Composite Double-Curved Omega Stringer
Deformation Prediction of Composite Bolted Joints Considering Multi-Source Variables
Experimental Study on Penetration Characteristics of Domestic Automated Placement Dry Fibers

Related Author

YUAN Yi
WANG Xiaolong
TAN Jingwen
MENG Jianan
LI Rui
YANG Xudong
XIA Hongda
WU Bin

Related Institution

Sino-European Institute of Aviation Engineering, Civil Aviation University of China
Engineering Techniques Training Center, Civil Aviation University of China
School of Aerospace Engineering, Huazhong University of Science and Technology
National Key Laboratory of Digital and Agile Aircraft Design
AVIC Xi’an Aircraft Design Institute
0